Curing finish.

Collapse
X
 
  • Time
  • Show
Clear All
new posts
  • nf1e
    Senior Member
    • Nov 2012
    • 2122

    #1

    Curing finish.

    Just hung a small batch of freshly unitized gas systems over the wood furnace for their 10 day curing. Welded them up yesterday and sprayed with Aluma-Hyde then set in the dryer at 90 degrees for 24 hours first, now for their final cure. Red on some is reflection off the wood. Whatta Hobby!

    gas cylinders 1.jpg
  • Allen
    Moderator
    • Sep 2009
    • 10580

    #2
    Well, this is the season for baking. Mostly people bake gingerbread men, fruit cakes and Christmas cookies but M14 unitized gas cylinders are another consideration.

    Thanks for the pics.

    Comment

    • nf1e
      Senior Member
      • Nov 2012
      • 2122

      #3
      At least these aren't too fattening.

      Comment

      • Allen
        Moderator
        • Sep 2009
        • 10580

        #4
        Originally posted by nf1e
        At least these aren't too fattening.
        Extra crunchy though.

        Comment

        • nf1e
          Senior Member
          • Nov 2012
          • 2122

          #5
          To the extreme, I would guess.

          Comment